• Login
    Search 
    •   MINDS@UW Home
    • MINDS@UW Eau Claire
    • UWEC Office of Research and Sponsored Programs
    • Search
    •   MINDS@UW Home
    • MINDS@UW Eau Claire
    • UWEC Office of Research and Sponsored Programs
    • Search
    JavaScript is disabled for your browser. Some features of this site may not work without it.

    Search

    Show Advanced FiltersHide Advanced Filters

    Filters

    Use filters to refine the search results.

    Now showing items 1-1 of 1

    • Sort Options:
    • Relevance
    • Title Asc
    • Title Desc
    • Issue Date Asc
    • Issue Date Desc
    • Results Per Page:
    • 5
    • 10
    • 20
    • 40
    • 60
    • 80
    • 100
    Thumbnail

    Nanoindentation of Silica Colloid Thin Films Sintered at Various Temperatures 

    Dunham, Douglas J.; Fiori, Mark; Baker, Grace; Knoke, Karen (2018-04)
    A Hysitron nanoindentor was used to test the hardness and reduced modulus of several two sample groups. These samples consisted of silica colloids deposited onto glass slides that were sintered at various temperatures. ...

    Contact Us | Send Feedback
     

     

    Browse

    All of MINDS@UWCommunities & CollectionsBy Issue DateAuthorsTitlesSubjectsThis CommunityBy Issue DateAuthorsTitlesSubjects

    My Account

    Login

    Discover

    Author
    Baker, Grace (1)
    Dunham, Douglas J. (1)
    Fiori, Mark (1)
    Knoke, Karen (1)Subject
    Chemistry (1)
    Hysitron nanoindentor (1)
    Posters (1)
    Silica colloids (1)
    ... View MoreDate Issued
    2018 (1)
    Has File(s)
    Yes (1)

    Contact Us | Send Feedback